DuPont de Nemours, Inc. · NYSE:DD

DuPont de Nemours — DuPont — Technical Presentation (January 2017)

24 slides from DuPont de Nemours's technical presentation, January 2017

  1. Slide 1: Kevlar Technical Sales Leader, Mechanical Protection

    Jill A. Clements DuPont™ Kevlar® Technical Sales Leader, Mechanical Protection January 2017

  2. Slide 2: Jill Clements Introduction

    Jill Clements Jill is a Senior Research Engineer with DuPont and has 18 years of Introduction experience in the development of new products and new applications and currently holds 14 patents. Of those 18 years with DuPont, Jill has been in the Kevlar® business for 15 years and has worked in a varie

  3. Slide 3: Confidential for training DuPont personnel

    © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  4. Slide 4: The Keys to Cut Resistance

    Steel or glass in the core The Keys to Cut Resistance • Cut resistance is a function of basis weight and material composition • Cut resistance can be increased by: • Increasing basis weight (14 oz/yd² Kevlar® better than 8 oz/yd² Kevlar®) • Using engineered yarns made with stainless steel wire or ya

  5. Slide 5: Global Recognition of Cut Standards

    Global Recognition of Cut Standards 5 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  6. Slide 6: © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These

    © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  7. Slide 7: Hand Protection Standards

    Hand Protection Standards • Standards are developed and used to specify test methods that replicate the threats potentially seen in a task • Standards usually refer to levels that are achieved by the product tested according to a certain test method • Why do we need standards? Don't we already have

  8. Slide 8: Hand Protection Standards

    Hand Protection Standards • ANSI/ISEA 105-16: American National Standard for Hand Protection Classification • ANSI: American National Standards Institute • ISEA: International Safety Equipment Association • US Standard only – is not a government regulation like OSHA • Indicates the mechanical, therm

  9. Slide 9: Why Were Changes Made?

    • Glove performance in the cut-resistant market has improved tremendously in recent years as new yarns and new technologies have been developed • Increased granularity is needed within the current level 4 range (1500-3499 grams) Why Were Changes Made? Both ANSI 4 1,600 grams 3,200 grams • The goal o

  10. Slide 10: What Are The Changes? – ANSI/ISEA 105

    • Key area of focus for the changes is the area of cut-resistance testing and classification What Are • ASTM F2992-15 The Changes? – • ASTM F1790 methods are no longer referenced ANSI/ISEA 105 • The move to a single test method will give more consistent ratings between glove manufacturers • There wi

  11. Slide 11: Move to single Test Method: TDM-100

    Move to single Test Method: TDM-100 • A new blade is required for each cut • The blade is moved across the sample once • The cut resistance is determined by the load required to cut a 20mm reference distance 11 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized dis

  12. Slide 12: What Are The Changes? – New Levels

    What Are The Changes? – New Levels 12 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  13. Slide 13: © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These

    © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  14. Slide 14: EN 388 (European Norm)

    EN 388 (European Norm) • Standard referenced throughout the entire EU • Government regulated • Gloves are marked with levels of mechanical performance only • Although a European standard, it is recognized globally 14 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authoriz

  15. Slide 15: Current EN 388 Test Equipment

    Current EN 388 Test Equipment • The blade is reused • The cut resistance measured is a ratio of performance of the sample to the performance of a control fabric (cotton canvas) • ISO 13997 is recommended instead for materials with higher cut performance 15 © 2017 DuPont. Confidential for training Du

  16. Slide 16: Inclusion of the TDM-100

    • The most significant change will be in regard to the acceptance of the Inclusion of the ISO 13997 (TDM) cut test method (accounts for dulling of blade in Coup Test) TDM-100 • The results will still be reported in Newtons, not grams • Levels achieved through the use of the TDM method will be letter

  17. Slide 17: What Are The Changes? – EN 388

    What Are The Changes? – EN 388 If Impact Protection is not measured, that digit is left blank. 17 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  18. Slide 18: What Are The Changes? – EN 388

    What Are The Changes? – EN 388 18 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  19. Slide 19: Coupe method cannot be used interchangeably

    EN 388 Coup Method ANSI/ISEA 105-16 & ISO 13997 Coupe method cannot be used interchangeably with ASTM & ISO 19 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPo

  20. Slide 20: What Are The Changes? – EN 388

    What Are The Changes? – EN 388 NO CORRELATION between Coup method and TDM-100 method 20 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  21. Slide 21: When Can I Compare EN to ANSI?

    When Can I Compare EN to ANSI? Only when TDM has been applied to both 21 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  22. Slide 22: When Can I Compare EN to ANSI?

    When Can I Compare EN to ANSI? Only when TDM has been applied to both 22 © 2017 DuPont. Confidential for training DuPont personnel and personnel of authorized distributors. These slides & their content cannot be used without the expressed written consent of DuPont.

  23. Slide 23: Summary

    • Both the ANSI/ISEA 105 and EN 388 Standards for the evaluation of cut-resistant materials have been updated • Most significant changes will be in regard to the: • Expansion of the ANSI/ISEA levels from 5 to 9 with more granularity above the 1500- gram level; new levels are prefaced with an "A" • A

  24. Slide 24: Information corresponds to our current knowledge

    This information corresponds to our current knowledge on the subject and may be subject to revision as new knowledge becomes available. It is your responsibility to investigate other sources of information on this issue that more appropriately addresses your product and its intended use. This inform