Dow Inc. · NYSE:DOW

Dow — Technical Presentation (October 2014)

43 slides from Dow's technical presentation, Oct 23, 2014

  1. Slide 1: One Component, Many Options: The Growing Role of Acrylics in Industrial Coatings

    One Component, Many Options: The Growing Role of Acrylics in Industrial Coatings October 23, 2014 Dow.com

  2. Slide 2: Agenda

    Agenda • Waterborne Acrylics 101: The Basics • Market Perspective ‒ Market background ‒ Trend analysis • Game Changing Technologies: Redefining the Limits ‒ Changing the way latexes interact with pigments ‒ Pushing the limits on VOC ‒ New hybrid technologies for 2K coatings • New Applications ‒ Insu

  3. Slide 3: Waterborne Acrylics 101: The Basics

    Waterborne Acrylics 101: The Basics

  4. Slide 4: What are Waterborne Acrylic Coatings?

    What are Waterborne Acrylic Coatings? • Paints and coatings based on WB acrylic polymers (acrylic latex or acrylic emulsion) • Non acrylic latex polymers (SBR and vinyl acetate) • Most commonly associated with architectural coatings, but are used in numerous industrial paints and coatings Two Types

  5. Slide 5: Why Use Acrylics in Paints and Coatings?

    Why Use Acrylics in Paints and Coatings? • Excellent resistance to ultraviolet light (UV), which translates into excellent exterior durability ‒ Color and gloss retention ‒ Maintain clarity ‒ Resistance to chalking • Toughness • Maintain flexibility and resistance to embrittlement • Resistant to gra

  6. Slide 6: Waterborne Acrylics in Industrial Coatings

    Waterborne Acrylics in Industrial Coatings Field-applied industrial maintenance coatings for metal and concrete Traffic and roadmarking paints Elastomeric roof coatings General industrial finishing Plastic coatings Concrete and metal roof tiles Fiber cement siding Wood and wood composite coatings: e

  7. Slide 7: Types of Waterborne Acrylic Coatings Available

    Types of Waterborne Acrylic Coatings Available Waterborne acrylic resins are used a variety of industrial maintenance and commercial architectural coatings: Primers • Wash primers • Anti-corrosive primers • Block fillers • Masonry primers Direct-to-substrate finishes • DTM finishes • Elastomeric wal

  8. Slide 8: Benefits & Challenges of Waterborne Acrylic Coatings

    Benefits & Challenges of Waterborne Acrylic Coatings Benefits Challenges  Low VOC = less impact on environment • Application window, i.e., length of  Low odor painting season  Less concern over worker exposure to • Drying rate dependent on humidity hazardous solvents • Reduced water resistance 

  9. Slide 9: Market Perspective

    = Market Perspective

  10. Slide 10: U.S. Coatings Market

    U.S. Coatings Market U.S. Coatings Market (Gallons Consumed) U.S. Coatings Market by Technology 2% 1% 4% 5% WB 24% SB 53% Special Purpose Powder 23% OEM 33% 55% 100% Solid Architectural E-coat Radcure 2011 Consumption WB by Segment • 1.4 Billion gallons • Architectural – 72% • Valuation of $23.1 Bil

  11. Slide 11: Industrial Maintenance Applications Using WB Acrylics

    Industrial Maintenance Applications Using WB Acrylics Commercial Storage tanks Bridges Railcars Metal Buildings Architectural Shipping Structural Water Towers Pipes Containers Steelwork 11

  12. Slide 12: Industrial Maintenance Market Technology Distribution

    Industrial Maintenance Market Technology Distribution Distribution by volume, total volume 52.1 MM gallons (2010) Other Alkyd 14% 12% WB Acrylic 24% Epoxy 35% Polyurethane 15% Source: US Paint & Coatings Market Analysis (2010 – 2015) 12

  13. Slide 13: Bridge

    Bridge Where Used? Steel and concrete bridges – primers and topcoats Often used over primers of other chemistry, e.g., Zn rich Specified and used by states such as CA, GA, NC, FL, etc. Key Attributes Low VOC Color and Gloss retention 1K ease of use Barrier properties – corrosion resistance 13

  14. Slide 14: Rail & Container

    Rail & Container Where Used? Boxcars, hopper cars, gondola cars – exterior DTMs Shipping containers – primers/topcoats Key Attributes Low VOC Fast dry Gloss Color and Gloss retention 1K ease of use Barrier properties – corrosion resistance 14

  15. Slide 15: Commercial Architecture

    Commercial Architecture Where Used? Interior and exterior walls – concrete, drywall DTMs for steel structures Roof coatings Interior floor coatings Key Attributes Low VOC, low odor Color and Gloss retention 1K ease of use Barrier properties – corrosion and water resistance Chemical / solvent resista

  16. Slide 16: Industry Specifications Based on Waterborne Acrylics

    Industry Specifications Based on Waterborne Acrylics SSPC Paint Standards • Paint # 23: Latex Primer for Steel Surfaces (revised 2013) • Paint # 24: Latex Exterior Topcoat for Steel Surfaces (currently under revision) DOT Steel Bridge Specifications • Various states such as CA, GA, NC MPI Examples •

  17. Slide 17: Key Trends and Drivers in Industrial Space

    Key Trends and Drivers in Industrial Space • Sustainability/Regulations ‒ Trend toward WB, high solids ‒ VOC/odor reduction ‒ Carbon footprint ‒ Human health & safety • Performance ‒ Surface compatibility ‒ Improved durability/resistance ‒ Extreme environment corrosion protection • Cost Effectivenes

  18. Slide 18: Game Changing Waterborne Acrylic Technologies

    Game Changing Waterborne Acrylic Technologies

  19. Slide 19: Game Changing Waterborne Acrylic Technologies

    Game Changing Waterborne Acrylic Technologies New developments in WB acrylic technology are pushing the limits of their performance. Redefining the interaction between polymer and pigment Pushing the limits on VOC New hybrid technology for 2K coatings 19

  20. Slide 20: Challenges of Improving Corrosion Resistance

    Challenges of Improving Corrosion Resistance Corrosion resistance in 1K thermoplastic acrylic DTM relies mainly on barrier properties of the film. Barrier properties are Redefine the Interaction dominated by… Between Polymer and Pigment • In WB coatings, we are generally • Quality of film formation

  21. Slide 21: Film Formation of Conventional Latex Paint

    Film Formation of Conventional Latex Paint Acrylic latex Application Pigment Polymer Diffusion 21

  22. Slide 22: Film Formation with Latex-Pigment Composites

    Film Formation with Latex-Pigment Composites • Optimizing pigment dispersion through formation of • latex-pigment Composite Particles in the wet state Composite particle formation 22

  23. Slide 23: Benefits of New Technology: Latex-Pigment Composites

    Benefits of New Technology: Latex-Pigment Composites Unique self-assembly mechanism defines the interaction with the pigment, and offers improvements in: – Corrosion resistance – Gloss – Gloss retention – Hiding – Adhesion to difficult metals 23

  24. Slide 24: Corrosion Resistance: Effect of Pigment Dispersion on Barrier Properties

    Corrosion Resistance: Effect of Pigment Dispersion on Barrier Properties 35 Day Salt Spray Exposure • 18 PVC gloss white DTM • No inhibitive pigments • One coat, 3 mil DFT • Blasted HRS (SSPC-SP 5) Conventional acrylic latex New technology: Latex-pigment composites 24

  25. Slide 25: Challenges of Lowering VOC Levels

    Challenges of Lowering VOC Levels Trend in maintenance coatings is towards lower VOC, e.g., SCAQMD limit for IM coatings is currently at 100 g/L. Challenges presented Market also wants when lowering VOC… higher performance… • Hardness • Gloss and Durability • Block and print resistance • Corrosion r

  26. Slide 26: Development Objectives for Low VOC Acrylic DTM Resin

    Development Objectives for Low VOC Acrylic DTM Resin Significant reduction in VOC: Capability of < 50 g/L • Anticipating future industrial coating regulations • DTMs are increasingly used in the architectural space Maintain (or improve) properties relative to higher VOC binders • Hardness properties

  27. Slide 27: Benefits of New Technology

    Benefits of New Technology WB Acrylic DTM with <50 g/L VOC VOC Dirt Pickup Resistance Gloss Humidity Resistance Gloss retention (7 wk QUV A) Adhesion to CRS Low temp coalescence Corrosion Resistance (1000 hrs) Block Resistance (1 day oven block) DTM-1 COM-1 COM-2 COM-3 27

  28. Slide 28: Block Resistance

    Block Resistance Hardness properties such as block resistance can be difficult to maintain when lowering VOC levels. 1 Day Block Resistance 8 7 6 5 4 3 2 1 0 Low VOC DTM Commercial #1 <200 VOC Commercial #2 <50 VOC Commercial #3 <100 VOC 1 Day, 30 min. Oven Block 1 Day, Room Temp. Block 28

  29. Slide 29: Corrosion Resistance

    Corrosion Resistance 1,000 Hours Salt Spray Exposure over Cold Rolled Steel Commercial DTM Commercial DTM #1 #2 New technology <200 VOC <50 VOC Commercial DTM 8% coalescent Stopped @ 576 Stopped @ 576 #3 < 50 g/L hours hours <100 VOC 29

  30. Slide 30: Challenges of Improving Performance of 2K WB Coatings

    Challenges of Improving Performance of 2K WB Coatings Current 2K WB coatings based on epoxy chemistry are used in industrial and commercial applications, but have some limitations. Challenges for epoxy- Challenges for epoxy- amine systems acrylic systems • Short pot life • Slow reaction (acid / epox

  31. Slide 31: Current 2K Waterborne Coatings

    Current 2K Waterborne Coatings Type I Type II Type III Part A Liquid epoxy resin (LER) WB epoxy dispersion WB acrylic latex Part B WB amine hardener WB amine hardener WB epoxy dispersion pre-dispersed pre-dispersed epoxy resin acrylic latex epoxy resin waterborne liquid epoxy resin waterborne curing

  32. Slide 32: New Technology: Acrylic-Epoxy Hybrids

    New Technology: Acrylic-Epoxy Hybrids pre-dispersed AEH hybrid resin O O O O O O waterborne curing agent O O MIXING Part A = Acrylic-Epoxy Hybrid Resin • Acrylic and epoxy in the same particle • Epoxy-functional • Colloidal properties similar to acrylic latex • EEW similar to SER (low 32

  33. Slide 33: Benefits of New Technology: Acrylic-Epoxy Hybrids

    Benefits of New Technology: Acrylic-Epoxy Hybrids <50 g/L VOC capability Long pot life (~ 4 – 10 hour pot life) Fast cure (amine-epoxy reaction) Fast dry time (lacquer dry of acrylic) Fast hardness development Good durability (due to acrylic) Low viscosities for easy 2K mixing (i.e., a latex system)

  34. Slide 34: Gloss Retention on UV Exposure

    Gloss Retention on UV exposure 100 90 80 60 Degree Gloss 70 60 50 40 COM-P3 30 AEH-P1 20 10 0 QUVA Exposure Time (Hours) Acrylic component facilitates improved UV durability 34

  35. Slide 35: New Applications for Waterborne Acrylics

    New Applications for Waterborne Acrylics

  36. Slide 36: New Applications for Waterborne Acrylics

    New Applications for Waterborne Acrylics Thermal Insulation Sound Damping Coatings Coatings 36

  37. Slide 37: Thermal Insulation Coatings: A New Way to Insulate

    Thermal Insulation Coatings: A New Way to Insulate • Insulation is used to prevent heat loss (or gain) ‒ Energy conservation ($) ‒ Process control ‒ Safety – personnel protection (e.g., from burns) • Formulated with WB acrylic resins and low thermal conductivity fillers • Applied using traditional c

  38. Slide 38: Energy Efficiency: Energy Use in a Model Scenario

    Energy Efficiency: Energy Use in a Model Scenario Energy consumption (kWh) to maintain various internal temperatures for a six-hour period with a 125 mil DFT insulation coating. 22 – 36% less energy No Coating used Internal Temperature IC-1002-1 180 F (hollow glass spheres) 250 F 325 F IC-1002-4 (si

  39. Slide 39: Benefits of Thermal Insulation Coatings

    Benefits of Thermal Insulation Coatings WB Acrylic binders facilitate easy formulation of thermal insulation coatings, which offer : ‒ Low thermal conductivity (k-value) ‒ Personnel protection (safe touch) ‒ Insulating properties / Energy management ‒ Energy savings ‒ Improved inspection for CUI ‒ E

  40. Slide 40: Sound Damping Coatings: Reducing Noise and Vibration

    Sound Damping Coatings: Reducing Noise and Vibration What is Liquid Applied Sound Damping? • The use of coatings to reduce sound and vibration • Typically used in the Automotive industry as a replacement for bitumen or asphaltic pads used on interior of body • Applied by airless spray Where else cou

  41. Slide 41: WB Acrylic Binder Design and Effect on Sound Damping

    WB Acrylic Binder Design and Effect on Sound Damping Range of Temperature Conditions and Performance Options Changes in Tg and other emulsion construction variables allow the tailoring of damping performance to individual specifications 41

  42. Slide 42: Benefits of Sound Damping Coatings

    Benefits of Sound Damping Coatings • Customizable solutions for sound damping • Applications Any application that can benefit from sound management and reduced noise, vibration and harshness (NVH): – Automotive (Passenger Car, Truck, Van) – Commercial Transportation (Marine, Rail, Bus) – Agriculture

  43. Slide 43: Conclusions

    Conclusions • Waterborne acrylics are one of the major technologies used in Industrial and Commercial Coatings • Wide range of compositions and corresponding performance is available • New advances are pushing the limits on performance, such as: ‒ Corrosion resistance ‒ VOC capability ‒ Improved bal