EcoSynthetix Inc. · TSX:ECO
EcoSynthetix — INDA's RISE 2011 Conference
29 slides from EcoSynthetix's conference presentation, Oct 5, 2011

Slide 1: Biolatex binders: Next generation breakthrough using nano-starch dispersions
INDA’s RISE 2011 Conference October 5, 2011 Biolatex® binders: Next generation breakthrough using nano-starch dispersions Dr. Alex Tseitlin EcoSynthetix Inc.

Slide 2: Polymers are Everywhere
2 Packaging Paints & Coatings Insulation Adhesives Printer Ink Coated Paper Personal Care Carpet Backing MDF(Particle Board) Polymers are Everywhere: commonly used in industrial manufacturing

Slide 3: Product Pipeline
3 Product Pipeline Feedstock Technology Platforms Products Markets >$60B Paint & Coatings Personal Care Starch BIOLATEX Polymer ECOSPHERE Paper & Paperboard Building Products Mining Inks & Toners Sugar ECOMER ECOSTIX Adhesives Surfactants

Slide 4: Biolatex Markets and Applications
4 Biolatex® Markets and Applications Technology Current Feedstock Markets Platforms Applications Building Products Fiberglass Insulation Fabrics & Textiles Roofing Shingles Starch BIOLATEX Polymer Paint & Coatings Filters Personal Care & Paperboard Disposables Packages Paper & Packaging Personal Gel

Slide 5: A new technology "S" curve in the making
5 A new technology “S” curve in the making Petroleum based polymers are reaching the end of their product improvement life cycle Biolatex® emulsions Advances: • Many new grades and Adoption & applications Economic Today • Towards 100% synthetic latex Value Added replacement Petroleum • Many other pr

Slide 6: Renewable inputs to biobased latex
6 Renewable inputs to biobased latex Renewable Water Innovative Technology Dry Feedstocks Chemistry Biopolymer Product

Slide 7: EcoSynthetix biopolymer nanoparticle technology
7 EcoSynthetix biopolymer nanoparticle technology 1. Renewable Inputs 2. Biolatex Product Produced by Green Manufacturing Process 15 µm 0.1 µm Starch biopolymers (corn, Proprietary process turns starch (soluble polymer) tapioca, potato, wheat, etc.) + into a biolatex® nanoparticle (insoluble polymer

Slide 8: Petroleum-based polymer prices
8 Petroleum-based polymer prices TOO HIGH TOO VOLATILE $160 $120 R2 = 0.84 $80 SB Latex price SB Latex $40 input $0 2004 2005 2006 2007 2008 2009 2010 2011 SB Latex: $/100 lbs Oil: $/barrel

Slide 9: Carbon footprint reduction of biolatex emulsions
9 Carbon footprint reduction of biolatex® emulsions Biolatex coated paper is not only sustainable it is compostable (biodegradable) and more recyclable (repulpable) Cradle-to-cradle carbon footprint reduction would be greater than 67% Petro-latex and biolatex binder Kg of CO2 Emitted per Kg of P

Slide 10: Production of oil-based latex via emulsion polymerization and biolatex binder
10 Production of oil-based latex via emulsion polymerization and biolatex binder Bottom Up Approach Top Down Approach a) SEM Scanning Electron Microscopy ESEM 15 µm (SEM), Environmental SEM (ESEM), and Scanning Transmission Electron Microscopy (STEM) Native Starch Granules Proprietary Process Synthe

Slide 11: Analysis of dry biolatex powder: agglomerate particles
11 Analysis of dry biolatex powder: agglomerate particles 1.20 HELOS Light Scattering Analysis o oo (dry agglomerate powder; vibrated gravity feed) o o 1.00 Volume x (10%) Mean Dia. x (50%) x (90%) % < 2 µm o (µm) (µm) (µm) (µm) o 315.6 70.6 275.3 627.3 0.05% o o Density Distribution 0.80 Dry biolat

Slide 12: Analysis of biolatex emulsion: biopolymer nanoparticles
12 Analysis of biolatex emulsion: biopolymer nanoparticles Dynamic Laser Light Scattering (DLS) Measurements 14 12 biolatex® dispersion (freeze dried) 10 8 0.1 µm (100 nm) 6 ESEM 4 2 0 1 nm 10 nm 100 nm 1 μm 10 μm 100 μm DLS of biolatex emulsion shows narrow particle size range: ~50-150 nm

Slide 13: Comparison of biolatex emulsion to other dispersions
13 Comparison of biolatex emulsion to other dispersions Petroleum-derived synthetic emulsions biolatex® SB Acrylic PVAc native corn nanoparticle emulsion Emulsion Emulsion Emulsion starch 10 nm 100 nm 1000 nm 10,000 nm 100,000 nm 1 µm 10 µm 100 µm Particle Size Measurements

Slide 14: Fundamental lab study on volume swell ratio
14 Fundamental lab study on volume swell ratio (from relative viscosity measurements at extremely low dilution)

Slide 15: Virtual density reduced from 1.6 to ~1
15 The film formation of water-swollen, crosslinked biopolymer nanoparticles Free-Flowing Aqueous dispersion of water- Dispersion swollen biopolymer nanoparticles Drying/Compaction Gelation/ Entanglement & insolubilization Immobilization at the particle interfaces Particle Deformation & Further Coal

Slide 16: Emerging biolatex emulsion technology
16 Emerging biolatex® emulsion technology

Slide 17: Biolatex Markets and Applications
17 Biolatex® Markets and Applications Technology Current Feedstock Markets Platforms Applications Building Products Fiberglass Insulation Fabrics & Textiles Roofing Shingles Starch BIOLATEX Polymer Paint & Coatings Filters Personal Care & Paperboard Disposables Packages Paper & Packaging Two recent

Slide 18: Formaldehyde free binder for fiberglass insulation
18 Formaldehyde free binder for binder for fiberglass insulation Fiberglass insulation Tensile strength test • Classic nonwoven fiberglass • Looked several binders application – Polyacrylic Acid • Market forces driving toward – Polyester “formaldehyde free” products – EcoSphere Biolatex – Combinatio

Slide 19: Tensile strength: blends with PAA
19 Blends with PAA Tensile strength 35 100 90 30 80 25 70 Max Load, kgF 60 20 50 Dry 15 Wet 40 Ret., % 10 30 20 5 10 0 0 PAA Eco/PAA50/50 Eco/PAA Eco/PAA Eco/PAA 60/40 75/25 50/50T

Slide 20: Tensile strength: blends with polyester
20 Blends with Polyester Tensile strength 30 88 86 25 84 20 82 Max Load, kgF 80 Dry 15 Wet 78 Ret., % 10 76 74 5 72 0 70 PE Eco/PE 50/50 Eco/PE 60/40 Eco/PE 75/25 Eco/PE 50/50T

Slide 21: Tensile strength – Comparison of binders
21 Tensile strength – Comparison of binders Tensile Strength 35 100 90 30 80 25 70 Max. Load, kgF 60 20 50 15 wet 40 dry 10 30 ret., % 20 5 10 0 0

Slide 22: SEM images
22 SEM images PF resin 50/50 blend of Ecosphere with PAA

Slide 23: Working with traditional formaldehyde binder for asphalt shingle
23 Working with tradition formaldehyde binder for binder for asphalt shingle Asphalt fiberglass Tensile strength test: shingle: • Combined with UF • Combination of Asphalt Resin and fiberglass • Compared against SB • Primary binder is urea- latex formaldehyde • Measured Tensile • Latex additives use

Slide 24: Hand sheet testing (wet laid glass fiber mat)
24 Hand sheet testing (wet laid glass fiber mat ) Tensile strength 40 96 94 35 92 30 90 88 Max Load, kgF 25 86 20 Dry 84 Wet 15 82 Ret., % 10 80 78 5 76 0 74 UF with 5% of SB UF with 5% of 2202 Eco UF with SB/Eco 1:3 UF with 5% of 2202* Eco* * EcoSphere is cooked-in (added during UF resin polymeriza

Slide 25: Biolatex Markets and Applications
25 Biolatex® Markets and Applications Technology Current Feedstock Markets Platforms Applications Building Products Fiberglass Insulation Fabrics & Textiles Roofing Shingles Starch BIOLATEX Polymer Paint & Coatings Filters Personal Care & Paperboard Disposables Packages • New applications being Pape

Slide 26: New Facility – Corporate HQ & Center of Innovation
26 New Facility – Corporate HQ & Center of Innovation Provides us with a State-of-the-Art Research facility for Product Development & Process Development Pilot Production Line: Laboratories and state-of-the-art pilot manufacturing equipment Maximum flexibility for R&D and rapid prototypi

Slide 27: Who we are & what we do
27 Who we are & what we do Founded in 1996 – Fundamental redesign concepts applied to agro-based materials to impart superior performance Technology leader – A broad and global patent portfolio: Composition-of-Matter/Process/Product/Application Performance at lower cost – Replacing petroleum based p

Slide 28: Corporate Overview
28 Corporate Overview We are a technology and market developer of biolatex® emulsions which are used to substitute petroleum-based products in a variety of industries. Society will benefit from our enterprise as a result of our products being sustainable, based on green chemistry and having a much l

Slide 29: Questions?
29 Thank you! Questions? Dr. Alex Tseitlin Atseitlin@ecosynthetix.com Phone: (289) 288-4734 EcoSynthetix®, EcoSphere®, and biolatex® are registered trademarks of EcoSynthetix Inc. For simplicity and convenience, the trademark symbol ® is not used in every instance. Note that we intend biolatex® be u
Source: Internet Archive copy of ecosynthetix.com
More decks from EcoSynthetix Inc.
Q2 2026 Earnings Presentation16 slides · Jul 29, 2026
Shareholder Meeting (May 2026)30 slides · May 21, 2026
Q1 2026 Earnings Presentation18 slides · May 6, 2026
Investor Presentation (March 2026)27 slides · March 2026
Q4 2025 Earnings Presentation16 slides · Feb 20, 2026
Q3 2025 Earnings Presentation15 slides · Nov 7, 2025